5. RESULTS
5.1 Unless otherwise specified in the detail specification, one specimen from each layer of tape taken for
test, 4.1, shall be tested.
5.2 The petrolatum resistance of the layer of tape shall be the result obtained from the specimen tested.
5.3 Any softness, tackiness, or brittleness of the varnish shall be recorded.
5.4 The temperature and time of exposure shall be recorded.